1. Automatic welding equipment will produce weld slag. The analysis of the price of automatic welding machine manufacturers is mainly due to the following three reasons:

After the bottom welding is not thorough, the slag at the root cannot be completely overflowed during the rapid heat welding.

The improper root cleaning method through root welding will cause the grooves on both sides of the root bead to be too deep and have a W-shape. In rapid thermal welding, the slag flowing into the deep groove is too late to overflow and form slag inclusions.

Too fast arc closing at the overhead welding position can easily cause slag inclusion.


2. Reasons for porosity in the welding process of automatic welding equipment:

When the cover surface is welded, the molten pool will overheat and absorb a large amount of surrounding air.

When welding the cover plate, the electrode swings too much and the molten pool is not well protected.

If the root gap is too small, it is easy to produce needle-shaped bubbles in the root.

The electrode is not used up within the specified time or is exposed to the air for a long time.

Automatic fiber laser welding machine price


3. Causes of cracks in the weld

If the construction site has large ups and downs and the mound is not buffered in time, the pipeline is under stress and stress cracks are prone to occur at the welding arc point (especially at 6 o'clock).

In the welding process, if the counterpart is loosened or evacuated as soon as possible, the molten iron in the molten pool will solidify in the future and cracks will easily occur in the welding arc.

Welders use improper arc collection methods, such as extinguishing the arc directly at the overhead welding position, which can lead to the formation of arc craters due to the incomplete filling of the molten pool and the appearance of arc crater cracks.


4. Causes of indentation during welding by automatic welding equipment

The penetration depth is not enough during the bottom welding.

The welding current is too large, and the welding speed is too slow during the heat welding process (5-7 points).